Abstract
The single-mode optical fibers were fabricated from TeO2-WO3-La2O3-(Bi2O3) glasses with low content of impurities and absorption losses less then 100 dB/km (1.56 μm). Rode-in-tube as well as monolith preform stretching techniques were used.
© 2011 Optical Society of America
PDF ArticleMore Like This
V. V. Dorofeev, A. N. Moiseev, M. F. Churbanov, V. G. Plotnichenko, A. F. Kosolapov, and E. M. Dianov
SOMC4 Specialty Optical Fibers (SOF) 2011
V. V. Dorofeev, A. N. Moiseev, I. A. Kraev, S. E. Motorin, A. F. Kosolapov, V. G. Plotnichenko, and D. V. Philippovskiy
STu3F.2 Specialty Optical Fibers (SOF) 2012
V.V Dorofeev, A.N. Moiseev, A.F. Kosolapov, V.G. Plotnichenko, S.V. Muraviov, M.Yu. Koptev, and A.V. Kim
JM5A.9 Bragg Gratings, Photosensitivity, and Poling in Glass Waveguides (BGPP) 2014