CaldeCast StrongLite TDS
CaldeCast StrongLite TDS
CaldeCast StrongLite TDS
TECHNICAL DATA
AVERAGE
PRODUCT PROPERTIES STANDARD UNITS
VALUES
CHEMICAL ANALYSIS
Calcined basis
PHYSICAL PROPERTIES
Measured on samples prepared according to EN 1402-5 -
Bulk density
after drying at 110 °C EN 1402-6 1.57 g/cm3
after firing at 800 °C EN 1402-6 1.40 g/cm3
Cold crushing strength
after drying at 110 °C EN 1402-6 25 MPa
after firing at 800 °C EN 1402-6 18 MPa
after firing at 1000 °C EN 1402-6 12 MPa
after firing at 1200 °C EN 1402-6 10 MPa
Permanent linear change
after firing at 800 °C EN 1402-6 -0.15 %
after firing at 1000 °C EN 1402-6 -0.35 %
after firing at 1200 °C EN 1402-6 -0.50 %
Thermal conductivity
at a mean temperature of 500 °C CALD 016 0.49 W/mK
at a mean temperature of 800 °C CALD 016 0.51 W/mK
at a mean temperature of 1000 °C CALD 016 0.54 W/mK
Reversible thermal expansion after firing at 1000°C - 0.6 %