Electric and magnetic polarizabilities of hexagonal Ln2CuTiO6 (Ln=Y, Dy, Ho, Er and Yb)
Authors:
Debraj Choudhury,
Abhijit Hazarika,
Adyam Venimadhav,
Chandrasekhar Kakarla,
Kris T. Delaney,
P. Sujatha Devi,
P. Mondal,
R. Nirmala,
J. Gopalakrishnan,
Nicola A. Spaldin,
Umesh V. Waghmare,
D. D. Sarma
Abstract:
We investigated the rare-earth transition metal oxide series, Ln2CuTiO6 (Ln=Y, Dy, Ho, Er and Yb), crystallizing in the hexagonal structure with non-centrosymmetric P63cm space group for possible occurrences of multiferroic properties. Our results show that while these compounds, except Ln=Y, exhibit a low temperature antiferromagnetic transition due to the ordering of the rare-earth moments, the…
▽ More
We investigated the rare-earth transition metal oxide series, Ln2CuTiO6 (Ln=Y, Dy, Ho, Er and Yb), crystallizing in the hexagonal structure with non-centrosymmetric P63cm space group for possible occurrences of multiferroic properties. Our results show that while these compounds, except Ln=Y, exhibit a low temperature antiferromagnetic transition due to the ordering of the rare-earth moments, the expected ferroelectric transition is frustrated by the large size difference between Cu and Ti at the B-site. Interestingly, this leads these compounds to attain a rare and unique combination of desirable paraelectric properties with high dielectric constants, low losses and weak temperature and frequency dependencies. First-principles calculations establish these exceptional properties result from a combination of two effects. A significant difference in the MO5 polyhedral sizes for M = Cu and M = Ti suppress the expected co-operative tilt pattern of these polyhedra, required for the ferroelectric transition, leading to relatively large values of the dielectric constant for every compound investigated in this series. Additionally, it is shown that the majority contribution to the dielectric constant arises from intermediate-frequency polar vibrational modes, making it relatively stable against any temperature variation. Changes in the temperature stability of the dielectric constant amongst different members of this series are shown to arise from changes in relative contributions from soft polar modes.
△ Less
Submitted 24 September, 2010; v1 submitted 2 June, 2010;
originally announced June 2010.
-
Correlation between extrinsic electroresistance and magnetoresistance in fine-grained La0.7Ca0.3MnO3
Authors:
P. Sujatha Devi,
A. Kumar,
Dipten Bhattacharya,
Shilpi Karmakar,
B. K. Chaudhuri
Abstract:
We report our observation of a correlation between the extrinsic electroresistance (EER) and magnetoresistance (EMR) via grain size in fine-grained La0.7Ca0.3MnO3. The nature of dependence of EER and EMR on grain size (~0.2-1.0 micron) indicates that for finer grains with low-resistive boundaries both of them follow similar trend whereas they differ for coarser grains with high-resistive boundarie…
▽ More
We report our observation of a correlation between the extrinsic electroresistance (EER) and magnetoresistance (EMR) via grain size in fine-grained La0.7Ca0.3MnO3. The nature of dependence of EER and EMR on grain size (~0.2-1.0 micron) indicates that for finer grains with low-resistive boundaries both of them follow similar trend whereas they differ for coarser grains with high-resistive boundaries. This could be due to a crossover in the mechanism of charge transport across the grain boundaries - from spin-depedent scattering process to spin-polarized tunneling one - as a function of grain size.
△ Less
Submitted 27 August, 2010; v1 submitted 22 August, 2008;
originally announced August 2008.
-
Ferromagnetism in nanoscale BiFeO3
Authors:
R. Mazumder,
P. Sujatha Devi,
Dipten Bhattacharya,
P. Choudhury,
A. Sen,
M. Raja
Abstract:
A remarkably high saturation magnetization of ~0.4mu_B/Fe along with room temperature ferromagnetic hysteresis loop has been observed in nanoscale (4-40 nm) multiferroic BiFeO_3 which in bulk form exhibits weak magnetization (~0.02mu_B/Fe) and an antiferromagnetic order. The magnetic hysteresis loops, however, exhibit exchange bias as well as vertical asymmetry which could be because of spin pin…
▽ More
A remarkably high saturation magnetization of ~0.4mu_B/Fe along with room temperature ferromagnetic hysteresis loop has been observed in nanoscale (4-40 nm) multiferroic BiFeO_3 which in bulk form exhibits weak magnetization (~0.02mu_B/Fe) and an antiferromagnetic order. The magnetic hysteresis loops, however, exhibit exchange bias as well as vertical asymmetry which could be because of spin pinning at the boundaries between ferromagnetic and antiferromagnetic domains. Interestingly, like in bulk BiFeO_3, both the calorimetric and dielectric permittivity data in nanoscale BiFeO_3 exhibit characteristic features at the magnetic transition point. These features establish formation of a true ferromagnetic-ferroelectric system with a coupling between the respective order parameters in nanoscale BiFeO_3.
△ Less
Submitted 17 May, 2007;
originally announced May 2007.
-
Orbital order-disorder transition in La(1-x)Nd(x)MnO(3) (x = 0.0-1.0) and La(1-x-y)Nd(yx)Sr(y)MnO(3) (x = 0.1; y = 0.05,0.1)
Authors:
Dipten Bhattacharya,
P. Sujatha Devi,
H. S. Maiti
Abstract:
The nature of orbital order-disorder transition has been studied in the La(1-x)Nd(x)MnO(3) (x = 0.0-1.0) series which covers the entire range between two end points - LaMnO(3) and NdMnO(3) - as well as in La(0.85)Nd(0.1)Sr(0.05)MnO(3) and La(0.8)Nd(0.1)Sr(0.1)MnO(3). It has been observed that the first-order nature of the transition gives way to higher order with the increase in "x" in the case…
▽ More
The nature of orbital order-disorder transition has been studied in the La(1-x)Nd(x)MnO(3) (x = 0.0-1.0) series which covers the entire range between two end points - LaMnO(3) and NdMnO(3) - as well as in La(0.85)Nd(0.1)Sr(0.05)MnO(3) and La(0.8)Nd(0.1)Sr(0.1)MnO(3). It has been observed that the first-order nature of the transition gives way to higher order with the increase in "x" in the case of pure manganites. The latent heat (L) associated with the transition, first, drops with a steeper slope within x = 0.0-0.3 and, then, gradually over a range 0.3<x<0.9. This drop could, possibly, be due to evolution of finer orbital domain structure with "x". In the case of Sr-doped samples, the transition appears to be of higher-order nature even for a doping level 5 at%. In both cases, of course, the transition temperature T(JT) rises systematically with the drop in average A-site radius <r(A)> or rise in average Mn-O-Mn bond bending angle <cos^2(phi)> while no apparent correlation could be observed with doping induced disorder sigma^2. The cooperative nature of the orbital order, therefore, appears to be robust.
△ Less
Submitted 7 December, 2004;
originally announced December 2004.