Hardness Conversion Chart

Sclerscope Diamond
Brinell Tensile Strength Hardness Rockwell Pyramid
Number Scale
Dia. Imp. Carbide Std Mpa Hardness "A" "C" HV10 HV30
Tons / 1000lb / kg /
for 10mm Ball Ball N/mm2 Number Scale Scale
inch2 Inch2 mm2
Ball
96 85.6 67.7 900
95 85 67 880
93 84.7 66.3 860
92 84.2 65.5 840
90 83.8 64.8 820
88 83.4 64 800
87 83 63.3 780
86 82.6 62.5 760
84 82.2 61.7 740
2.44 630 82 81.8 61 725
2.45 627 81.5 60.5 710
2.5 601 132 295 208 2039 81 81.2 60 698
2.55 578 127 284 200 1961 78 80.6 58.9 670
2.6 555 122 273 192 1884 75 79.6 57.1 630
2.66 534 117 262 184 1807 73 79 56.1 609
2.7 514 112 250 176 1729 71 78.2 54.4 572
2.75 495 495 108 241 170 1668 68 76.9 51.9 532
2.8 477 477 105 235 165 1621 66 76.3 50.7 517
2.85 461 461 101 226 160 1559 64 75.5 49.5 497
2.9 444 444 98 219 155 1513 62 74.2 47.5 470
2.95 429 429 95 212 150 1467 60 73.5 46 452
3 415 415 92 206 145 1420 58 73 44.8 437
3.05 401 401 88 197 139 1359 56 72.5 43.7 422
3.1 388 388 85 190 134 1312 54 71.5 42.4 408
3.15 375 375 82 183 129 1266 52 71 41.3 395
3.2 363 363 80 179 126 1235 51 70.3 39.9 381
3.25 352 352 77 172 121 1189 49 69.8 38.8 370
3.3 341 341 75 168 118 1158 48 69.2 37.7 359
3.35 331 331 73 163 114 1127 46 68.8 36.7 349
3.4 321 321 71 159 111 1096 45 68 35 337
3.45 311 311 68 152 107 1050 43 67.5 34 327
3.5 302 302 66 147 104 1019 42 66.8 33 318
3.55 293 293 64 143 101 988 41 66.2 32 308
3.6 285 285 63 141 99 973 40 65.7 30.9 300
3.65 277 277 61 136 96 942 38 65.2 29.8 292
3.7 269 269 59 132 93 911 37 64.6 29 284
3.75 262 262 58 130 91 895 36 64 27.5 275
3.8 255 255 56 125 89 865 35 63.6 26.6 269
3.85 248 248 55 123 87 849 34 62.9 25.2 261
3.9 241 241 53 118 84 818 33 62.6 24.3 255
3.95 235 235 51 114 81 787 32 62 23 247
4 229 229 50 112 79 772 31 61.6 22 241

Page 1 of 2
Hardness Conversion Chart
Sclerscope Diamond
Brinell Tensile Strength Hardness Rockwell Pyramid
Number Scale
Dia. Imp. Carbide Std Mpa Hardness "A" "C" HV10 HV30
Tons / 1000lb / kg /
for 10mm Ball Ball N/mm2 Number Scale Scale
inch2 Inch2 mm2
Ball
4.05 223 223 49 110 77 756 30 60.7 20.8 234
4.1 217 217 48 107 76 741 228
Hardness
"B" Scale
4.15 212 212 46 103 73 710 29 98 222
4.2 207 207 45 101 71 695 28 97 218
4.3 197 197 43 97 68 664 27 96 212
4.4 187 187 41 92 65 632 25 93 196
4.5 179 179 39 88 62 602 91 188
4.6 170 170 36 81 57 556 24 88.5 178
4.7 163 163 35 78 55 540 86 171
4.8 156 156 34 76 54 525 23 84.2 163
4.9 149 149 32 72 51 494 82 156
5 143 143 31 69 49 479 22 80 150
5.1 137 137 30 67 48 463 21 77 143
5.2 131 131 29.5 66 47 455 20.5 75 137
5.3 126 126 29 65 46 448 20 72.5 132
5.4 121 121 28 63 44 432 70 127
5.5 116 116 26 58 42 401 15 67 122

Page 2 of 2