WELDING INSPECTION REPORT

Inspection Date : WIR No. :


Project : Shift : Day Night
Product Type : Type of Finished : Bare Galvanized

Visual Inspection
Item Joint Welding Voltage Ampere REMARKS
Description ID No. Arc Welder’s Name STATUS
No. No. Crack Undercut Overlap Undersize Spatter Porosity Process Range Range (J.O. No., etc.)
Strike

Visual Inspection Acceptance Criteria (AWS D1.1/D1.1M Structural Welding Code – Steel): LEGEND :
1. Any crack shall be unacceptable, regardless of size or location. V.I. - Visual Inspection
2. Thorough fusion shall exist between adjacent layer of weld metal and between ACC. - Accepted
weld metal and base metal.
3. All craters shall be filled to provide the specified weld size.
4. Undersize portion of the weld shall not exceed 10% of the weld length.
5. Undercut shall be no more than 1mm deep.
6. CJP groove weld in but joints transverse to the direction of computed tensile
stress shall have no piping porosity.

Inspected by : Marco Antonio Marasigan Checked by : Acknowledge by : Noted by :


Certified Welding Inspector Welding Inspector (PWS) Site Engr./Leadman/Foremen QA/QC Supervisor