This test report summarizes compression testing of a bearing pad sample. The sample, measuring 387.0x235.0x47.54mm, was subjected to short and long duration compression tests using a SHIMADZU machine. After applying a test load of 90.00 M-Tons, a visual and physical inspection found no signs of failure such as cracking or chipping in the sample.
This test report summarizes compression testing of a bearing pad sample. The sample, measuring 387.0x235.0x47.54mm, was subjected to short and long duration compression tests using a SHIMADZU machine. After applying a test load of 90.00 M-Tons, a visual and physical inspection found no signs of failure such as cracking or chipping in the sample.
This test report summarizes compression testing of a bearing pad sample. The sample, measuring 387.0x235.0x47.54mm, was subjected to short and long duration compression tests using a SHIMADZU machine. After applying a test load of 90.00 M-Tons, a visual and physical inspection found no signs of failure such as cracking or chipping in the sample.
This test report summarizes compression testing of a bearing pad sample. The sample, measuring 387.0x235.0x47.54mm, was subjected to short and long duration compression tests using a SHIMADZU machine. After applying a test load of 90.00 M-Tons, a visual and physical inspection found no signs of failure such as cracking or chipping in the sample.