Location via proxy:   [ UP ]  
[Report a bug]   [Manage cookies]                

AZS - TC Aditi Cera 16 Dec 16681

Download as pdf or txt
Download as pdf or txt
You are on page 1of 1

CSIR-Central Glass & Ceramic Research Institute

(COUNCIL OF SCIENTIFIC & INDUSTRIAL RESEARCH )


NARODA CENTRE, NARODA INDUSTRIAL ESTATE, AHMEDABAD-382 330 (INDIA)

TEST CERTIFICATE
20162411-222 24/11/20J6. NQ . GC/NC/1382S/
Sample Regn. No.
M/s Aditi Cera Minerals GC/NC/TST-Misc/2016
Issued to 104/2, GIIDC Palej- 392 220. Ref. No. :
-th
Dist. Bharuch 16m Dec., 2016
Date :
Nil, dated 10.11.2016
Customer Ref. No. with Date :
SAMPLE DESCRIPTION AS PER : Refractory sample as submitted by the party.
CUSTOMERS LETTER

VISUAL OBSERVATION :Yellowish and off white granules.

TEST DESIRED

S. No. TEST
1. Determination of ZrO2, SiO2, TiO2, AI2O3, Fe203, CaO,
MgO, Na2O, K2O & LOI contents only.

RESULTS

Results
Constituents (%)

Si02 15.09
AI203 47.53
ZrO2 35.02
Fe203 0.10
Ti02 0.12
CaO 0.22
MgO 0.16
Na20 1.19
K20 0.16
LOI 0.25

Verified by

Signature :

Name : Dr. A.K. Chakraborty

Designation : Sr. Tech. Officer (3)

Authorized Signatory

Signature :
Name : Dr. SatV^fldra Nat
Designation : Scientist-in-Charge

This report refers only to the particular sample(s) submitted for test/calibration and the sample(s) was /were not drawn by us. This report may not be reproduced except in full, unless written