LORUS (Onstream)
LORUS (Onstream)
LORUS (Onstream)
Fluid loading
Θ Annular plate
Floor plate
Hidden corrosion at hard-to-access locations often poses inspectors for great problems.
Full inspection often requires taking components out of service for access; this is a
time consuming and costly procedure. LORUS has been developed to detect hidden
corrosion over a considerable range from a single access point. In a number of
applications, LORUS may be considered for on stream component inspection.
QUALITY SERVICES
Making the invisible visible
7332 rev. 1
Severity classification • poor annular plate condition may decrease
To a limited extent, corrosion severity may be the inspection range
estimated from the LORUS images. Reference
reflectors are used for reflectivity reference to Validation
give a rough depth indication in a few Various international trials for leading tank
severity grades. operators show the added value of LORUS
inspection. Feedback from invasive
Performance inspections shows good agreement. Further
• range up to 1 metre validation of LORUS is in progress.
• suitable for any tank diameter
• suitable for annular plates in thickness Integral inspection packages
range of 6 to 25 mm LORUS may be part of on and off stream
• able to detect severe (pitting) corrosion tank inspection packages. For on stream
• able to detect local gradual corrosion inspection, a combination of LORUS with
• corrosion mapping and area estimation visual inspection, magnetic flux leakage wall
• production 10 -15 metres per day thickness mapping, ultrasonic wall thickness
• suitable for corrosion growth monitoring mapping or other on stream techniques
• reflectivity of corroded areas may be used provides useful information about tank
to estimate severity condition without the need to open the tank.
LORUS may be applied to cover the floor
Restrictions region directly behind the tank shell and the
• no complete coverage of the tank floor corner weld, which are hard to access with
(the outer ring only) standard techniques.
• no discrimination between top and reverse
side corrosion is possible LORUS sometimes is applied to prioritise off
• the scanning surface must be free of stream inspection.
impurities, welding droplets, surface
corrosion and coating (well bonded paint
or coating is acceptable)
QUALITY SERVICES
Making the invisible visible