1. The minimum length of an intermittent fillet weld

A. 1"

B. 1 1/4"

C. 1 1/2"

D. 1 3/4"

2. How many times may a low hydrogen electrode be re-baked?

A. Not limited

B. Twice

C. Once, only after a 2 hour holding period

D. Once

3. Fillet weld end return lengths have a maximum requirement of ___________ times the nominal size
of the weld

A. 1 1/2

B. 4

C. 2

D. 3

4. What is the major function of the coating on an arc welding electrode?

A. Acts as a scavenger, removes oxides and impurities

B. Influences incomplete penetration

C. Liquefies the base metal

D. Adds moisture and accelerates the cooling rate


LA City Welder certification
Closed book Test. 1
5. Square wave refers to the ____________.

A. shape of the filler metal

B. shape of the tungsten electrode

C. shape of the output power

D. shape of the power source control box

6. What NDE process is indicated in the following description? Detects surface discontinuities only. It can
also verify fit-up, joint configuration, weld dimensions and profiles.

A. PT

B. RT

C. MT

D. VT

7. Of the following which is not considered a joint?

A. Lap

B. Corner

C. Groove

D. Edge

8. The Los Angeles City certified welding license must be renewed every _________?

A. 6 months

B. 1 Year

C. 2 years
LA City Welder certification
Closed book Test. 1
D. 3 years

9. Which of the following electrode(s) need shielding gas?

A. E71T-1

B. E71T-2

C. E71T3

D. Both E71T-1 and E71T-2

10. Arc strikes on the base metal shall be

A. Allowed on plate, not allowed on pressure pipe

B. Repaired with grinder

C. Allowed

D. Avoided

11. Field welding shall not be performed when the ambient temperature is

A. Lower than 0 degrees F

B. Above 0 degrees F

C. Over 120 degrees F

D. Below 102 degrees F

12. D1.1 structural code covers applications regarding carbon & low alloyed steels with a minimum yield
strength of?

A. Not covered in the D1.1 structural code

B. 100 KSI or less


LA City Welder certification
Closed book Test. 1
C. No limit

D. 100 KSI or more

13. Welding out of position with an EXX2X rod can cause?

A. Spatter

B. Overheating

C. Incomplete penetration

D. Undercut

14. A break in the arrow shaft of a weld symbol would have significance in a ______________?

A. Bevel or j-groove

B. None

C. Bevel only

D. J-groove only

15. When using the SMAW process the electrode is positive only when using?

A. DCSP

B. AC

C. NEVER

D. DCRP

16. Low hydrogen electrodes end in what digits?

A. 4, 7, 8

B. 8, 6, 1
LA City Welder certification
Closed book Test. 1
C. 5, 6, 8

D. 3, 4, 7

17. The "S" in ERXXS-X wire represents?

A. Selected

B. Silicone

C. Solid

D. Stainless

18. Omitted.

19. What electrode is deep penetrating, can be used in all positions and can only be used on DCRP?

A. E6013

B. E7018

C. E6011

D. E6010

20. What suffix numbers in FCAW electrodes indicate the need for shielding gas?

A. 1-6

B. 7-11

C. 1, 2, 5

D. 5, 6, 8

21. All prequalified WPS shall be prepared by the ___________?

A. Both a & b
LA City Welder certification
Closed book Test. 1
B. Contractor/fabricator

C. Welder

D. Inspector

22. All welding symbol information referring to the arrow side of the joint is found?

A. Below the reference line

B. Above the reference line

C. To the left of the welding symbol

D. In the tail

23. D1.5 is the ______________Code.

A. Structural Steel

B. Reinforcing Steel

C. Sheet/Light Gage

D. Bride Welding

24. What is the maximum fillet weld size for 7/16" thick lap joint?

A. 1/16"

B. 1/4"

C. 3/8"

D. 5/16"

25. The legend for figures 3.2 & 3.3 does not cover?

A. Preheat & interpass temperature


LA City Welder certification
Closed book Test. 1
B. Base metal thickness & penetration

C. Joint information

D. Backing information