MECHANICAL DATA
Tensile Modulus (ASTM D638) 448,000 psi (3.1 GPa) 440,850 psi (3.0 GPa)
Tensile Strength (ASTM D638) 8,140 psi (56.1 MPa) 7,910 psi (54.5 MPa)
Elongation (ASTM D638) 6% 6.5
Flexural Modulus (ASTM D790) 390,000 psi (2.7 GPa) 409,670 psi (2.8 GPa)
Flexural Strength (ASTM D790) 11,850 psi (81.7 (MPa) 11,100 psi (76.5 MPa)
Compression Strength (ASTM D695) 12,380 psi (85.4 MPa) 10,860 psi (74.9 MPa)
Tg Ultimate (DSC, midpoint) 123ºF/51ºC 127ºF/52ºC
Hardness (Shore D) 70-80 70-80
PROCESSING DATA
Mix Ratio (by volume) 2:1 2:1
Mix Ratio (by weight) 100:43 100:42
Viscosity (A/B/Mixed @ 77ºF/25ºC) 2160/30/370 2160/15/270
Component Density (specific density @ 77ºF/25ºC) 1.13 (resin), 0.98 (hardener) 1.13 (resin), 0.95 (hardener)
Mixed Density (specific density @ 77ºF/25ºC) 1.08 1.07
Pot Life (@ 77ºF/25ºC) 90 min 360 min
Tack Free Time (@ 95ºF/35ºC) 24 hrs 72 hrs
Recommended Full Cure 7 days @ 77ºF/25ºC, 7 days @ 77ºF/25ºC,
Post cure recommended Post cure recommended
ENVIRONMENTAL
DATA
VOC Content (ASTM D2369) 0.08 lbs/gal (9.2 g/L) 0.07 lbs/gal (8.0 g/L)
Mixed Biobased Carbon Content (ASTM D6866) 20% 20%