The document discusses various standards for steel composition and properties including IS 2062, IS 6240, IS 3039 and IS 1786.

IS 2062 and IS 3039 specify different grades of structural steel with restrictions on chemical elements like carbon, manganese, sulphur and phosphorus.

IS 2062, IS 3039 and IS 1786 specify minimum requirements for tensile strength, yield strength and elongation for different grades of structural and reinforced steel.

THINK!

- MARYLAND METRICS - The One-Stop Source For Metric And British Sized Fasteners, Wrenches, Cutting, & Measuring Tools, Metal Shapes, Oil Seals, O-Rings, Mechanical Power Transmission Equipment, Bearings, Hydraulic And Pneumatic Fittings & Tubing, Workholding Components, Plumbing Fittings, & Some Electrical & Electronic Components. Click to go to Maryland Metrics home page

Chemical Composition And Mechanical Properties of Steel (Indian Standard)


Grade I II III IV V Grade I II III IV V IS : 10748 - Specification Of Hot Rolling Steel Strips For Welded Tubes & Pipe CHEMICAL COMPOSITION C% Max Mn % Max. S% Max. 0.10 0.12 0.16 0.20 0.25 UTS ( Min.) Mpa 290 330 410 430 490 0.50 0.60 1.20 1.30 1.30 MECHANICAL PROPERTIES YS ( Min.) Mpa 170 210 240 275 310 0.05 0.05 0.05 0.05 0.05 P% Max. 0.05 0.05 0.05 0.05 0.05

EI. % ( Min. ) 5.65 Sqrt (So) 30 28 25 20 15

IS : 6240 HR - Steel Plate, Sheet and Coil for LP CHEMICAL COMPOSITION Constituent Carbon, Max. Manganese, Min Silicon, Max. Sulphur, Max. Phosphorous, Max. Aluminium, Min MECHANICAL PROPERTIES Property Tensile Strength Mpa (kgf/mm) Yield Strength. Mpa ( Kg/mm) Min Elongation, Min percent on guage length 5.65 OSo Bend EC v ( for 2.80-3.15 mm thickness) min * Both longitudinal and transverse directions.

Percent 0.16 0.30 0.25 0.030 0.030 0.02 Grade * 350 to 450 ( 36 to 46 ) 240 (25) 25 t 13.5

TOLERANCE AS PER IS : 513 Tolerance on Thickness of Sheets Tolerance on the thickness for different width Nominal Thickness Upto 0.25 Upto 1250 mm +/- 0.03 Above 1250 Upto 1600 Above 1600 -

Above 0.25-0.40 Above 0.40-0.60 Above 0.60-0.80 Above 0.80-1.00 Above 1.00-1.25 Above 1.25-1.60 Above 1.60-2.00

+/+/+/+/+/+/+/-

0.04 0.05 0.06 0.08 0.09 0.11 0.12

+/+/+/+/+/+/-

0.06 0.07 0.09 0.10 0.12 0.14

+/+/+/+/+/0.08 0.10 0.12 0.14 0.16

Tolerance on Width Of Sheets Width of Sheets Upto 1250 mm Above 1250 mm Tolerance +7 +10 -0 -0

Tolerance on Length of Sheets Length Upto 2000 mm Above 2000 mm Tolerance +15 +0.75 % of the length -0 -0

Chamfer Tolerance For Coils and Cut Length Form Coil Cut Length Tolerance 20 mm in any 5000 mm length 0.4% X length

Thickness Upto 0.63 Above 0.63-1.25 Above 1.25

Standard Flatness Tolerance for cut lengths Tolerance on specified width Upto 1200 Above 1200 - Upto 1500 15 18 12 15 10 12

Above 1500 22 19 17

Thickness Upto 0.63 Above 0.63-1.25 Above 1.25

Special Flatness Tolerance for Cut lengths Roller Levelled and Stretcher Levelled Tolerance on specified width Upto 1200 Above 1200 Upto 1500 6 7 5 6 4 5

Above 1500 8 7 6

Grade A B C Grade A B C

C% Max. 0.23 0.22 0.20 UTS(MPa) Min. 410 410 410

IS : 2062 - Specification of Steel for General Structural Purposes CHEMICAL COMPOSITION Mn% Max. S% Max. P% Max. Si% Max. 1.50 0.050 0.050 0.40 1.50 0.045 0.045 0.40 1.50 0.040 0.040 0.40 MECHANICAL PROPORTIES Y.S.(MPa) Min. 250 250 250 240 240 240 230 230 230 El.% Min. 5.65 Sqrt(So) 23 23 23

C.E.% Max. 0.42 0.41 0.39 Bend Test 3T 2T & 3T * 2T

* 2T - <= 25mm * 3T - > 25mm

Grade I II III Grade I II III

IS : 3039 - Specification of Structural Steel for Ship Building CHEMICAL COMPOSITION C% Max. Mn% S% Max. P% Max. Si% Max. 0.23 * 0.040 0.040 ** 0.21 0.70-1.4 0.040 0.040 0.10-0.35 0.18 0.70-1.5 0.040 0.040 0.19-0.50 MECHANICAL PROPERTIES Y.S. (MPa) Min. UTS (MPa) < 25 mm. > 25 < 50 mm. 400-490 230 220 400-900 235 235 400-490 235 235

Al% Min. 0.01 0.015 EI.% Min. 5.65 Sqrt (So) 22 22 22

IS : 1786 - High Strength Deformed Steel Bars and Wires for Concrete Reinforcement CHEMICAL COMPOSITION Constituent SAIL TMT 415 Carbon Sulphur Phosphorus Sulphur and Phosphorus Corrosion Resistant Elements Carbon Equivalent Property Fe 415 0.2 percent proof stress/yield stress Min 415 N/mm.sq. Elongation.percent ,Min,on gauge length 5.65.Square Root(A) 14.5 where A is the crosssectional area of the test piece Tensile Strength,Min. 10% more than the actual 0.2% proof stress but not less than 48.5 N/mm.sq. SAIL TMT 415 415 0.25 0.05 0.05 0.10 Percent, Maximum SAIL TMT 550 0.25 0.05 0.05 0.10 SAIL-TMT(Fe 415/FE 500/Fe 550) Fe 500 0.30 0.055 0.050 0.10 0.20 0.045 0.045 0.09 0.75 min 0.53 max

Fe 415 0.30 0.06 0.06 0.11 -

SAIL TMT 500 0.25 0.05 0.05 0.10 -

Fe 500 0.30 0.055 0.055 0.105 -

MECHANICAL PROPERTIES Grade SAIL Fe TMT 500 500 500 500 550

Fe 550 550

SAIL TMT 550

22(Up to 28mm dia) 20 12 (Above 28 mm dia) 10% more 8% more than than the actual actual 0.2% 0.2% proof proof stress stress but not but not less less than 500 than 545 N/mm.sq. N/mm.sq.

20(Up to 28mm dia) 18 8 (Above 26 mm dia) 8% more than the actual 0.2% proof stress but not less than 580 N/mm.sq. (Upto 28mm dia) & 560 N/mm.sq.) (above 28 mm dia) 6% more than the actual 0.2% proof stress but not less than 585 N/mm.sq.

18(Upto 25 mm dia) 16(Above 28 mm dia) 6% more than the actual 0.2% proof stress but not less than 630 N/mm.sq. (Upto 28mm dia) & 610 N/mm.sq.

(Upto 28mm (above 28 mm dia) dia) & 560 N/mm.sq.) Upto 28mm dia) & 560 N/mm.sq.) (above 28 mm (above 28 mm dia) dia)

SPECIFICATION FOR WIRE RODS


Chemical Composition Specifications Structure Quality Wire Rods Drawing Quality Wire Rods Low Carbon Drawing Quality Wire Rods Electrode Quality Wire Rod Grade IS2062 Grade A SWR-14 SWR-10 SAE-1008 IS-2879 Rimming Grade %C 0.23 max 0.14 max 0.08-013 0.1 max 0.1 max 0.1 max %Mn 1.50 max 0.60 max 0.30-0.60 0.6 max 0.3 max 0.38-0.62 %S 0.05 max 0.05 0.05 0.04 0.05 0.03 max max max max max %P 0.50 max 0.05 0.04 0.04 0.04 0.03 max max max max max Mechanical Properties Yield Tensile Elongation Mpa Mpa % 250 min 410 min 23 min -

Grade O D DD EDD Grade O D DD EDD

IS:1079-Specification of Hot Rolled Carbon Steel Sheets & Strips CHEMICAL COMPOSITION C% Mn % S% P% Max Max Max Max 0.15 0.60 0.055 0.055 0.12 0.50 0.04 0.04 0.10 0.45 0.035 0.035 0.08 0.40 0.030 0.03 MECHANICAL PROPERTIES UTS YS(Min.) EI.% Min. MPa MPa Lo-80 mm b-20 mm 28 260-390 32 260-380 36

Specification

Chemical composition (max) Tensile Strength Min. Mpa 410 410 440-560 440-560 490-610 540-660 540-660

Mechanical Properties Yield Strength Min. Mpa 240 240 300 300 350 410 410 % Elongation guage length 5.65 So 23 23 20 21 20 19 20 Maximum for all . .

C IS-2062 Gr A (SK) IS-2062 Gr B (SK) SAIL-MA 300 SAIL-MA 300 HI SAIL-MA 350 SAIL-MA 350 HI SAIL-MA 410 0.23 0.20 0.25 0.20 0.25 0.20 0.25

Mn 1.5 1.5 1.5 1.5 1.5 1.5 1.5

S 0.050 0.045 0.055 0.040 0.040 0.040 0.040

P 0.050 0.045 0.055 0.040 0.040 0.040 0.040

Nb+V+T 0.20 .

THINK!- MARYLAND METRICS - The One-Stop Source For Metric And British Sized Fasteners, Wrenches, Cutting, & Measuring Tools, Metal Shapes, Oil Seals, O-Rings, Mechanical Power Transmission Equipment, Bearings, Hydraulic And Pneumatic Fittings & Tubing, Workholding Components, Plumbing Fittings, & Some Electrical & Electronic Components. Click to go to Maryland Metrics home page
Phones: (800) 638-1830 or (410) 358-3130 are available Monday-Friday 8:30 AM to 5:30 PM Eastern time. Faxes: (800) 872-9329 or (410) 358-3142 & E-mail are available anytime. Warehouse & showroom hours are Monday-Friday 10 AM to 5:30 PM. [ To: Maryland Metrics home page ] [ To: Maryland Metrics Product Guide ] [ e-mail to Maryland Metrics ]

Please note that all Trademarks and Tradenames are the property of their respective owners. copyright 2000, 2009, 2011 maryland metrics -- all rights reserved -- ver gg22a chempropi.htm

You might also like