60.210
PREPARATION
All bases should be straight and in-line with no
variation greater than inch in ten feet
Surfaces must be cleaned and inspected for any
substance that will act as a bond-breaker
Concrete masonry units must be fully grouted,
open-textured with joints cut flush, not tooled
Substrates should be fully cured, dry and carrying
the design dead load prior to the application of the
plaster
A surface-applied bonding agent conforming to
ASTM C932 may be used as needed to insure a
good chemical bond and equalize suction porosity
throughout the entire face of the masonry
Cast-in-place concrete work: provide sufficient
abrasion for a proper mechanical bond with the
plaster
o The plastering contractor must verify the
type of bond-breaker used prior to direct
application of plaster. Sodium silicate bond
breakers will dissipate and can be plastered
without lath, however, petroleum, oil or
paraffin-based bond breakers do not
dissipate and good bond cannot be
guaranteed.
Apply metal lath when form oil, paint or other bond
breaking material is present
Overall performance of the plaster can be expected
to diminish when the unwarranted use of bondbreaking water-resistive barriers are incorporated