Stainarc 309L-17 (Rev 1)

Download as pdf or txt
Download as pdf or txt
You are on page 1of 1

Descriptions and Applications AWS A5.

4 E 309L-17
Rutile type low carbon MMA electrode for joining dissimilar steels (austenitic EN 1600: E 23 12 L R 32
to ferritic steels) and for cladding of austenitic steels. Weld metal consists of Werkstoff Nr: 1.4332
austenite with approx.15% delta ferrite. Cladding on unalloyed and low-alloy
steels are corrosion resistant in the first layer.

Good fusion of joint faces, finely rippled bead surface, easy slag removal, ↘ Welding Position ↙
excellent arc striking and re-striking.

Base Materials
Stainless steels for general use and for high temperature applications:
UNS Alloy EN Material Nᵃ UGINE
S30900 309 X15CrNiSi 20-12 1.4828 UGINOX R20-12
S30453 304LN X2CrNiN 18-10 1.4311
S30908 3098 X12CrNi23-13 1.4833 UGINOX R24-13S
X1OCrSiG 1.4712
X10CrA1 18 1.4742

All Weld Metal Mechanical Properties (Typical)


Tensile Strength Elongation
ISO – V J RT
Rm (N/mm²) %
600 >35 60

Typical Weld Metal Chemical Composition (%)


C Si Mn Cr Ni Mo S P

0.03 0.90 0.90 23.80 12.80 0.10 0.012 0.012

Amperes (A)
2.00mm 2.60mm 3.20mm 4.00mm 5.00mm

25-50 60-80 80-120 110-150 150-180

Welding Instruction ≈ Re-drying 1 hour at 250°C if necessary. Inter pass temperature: < 200°C.